Hi,

I am building a home with a builder and during the framing I found many studs that were cracked a lot. Builder pushed back on fixing these.
Need your input. Please see the attached pics. Like that there are several.
 

Attachments

  • Stud_Issue_4.jpg
    Stud_Issue_4.jpg
    2.5 MB · Views: 78
  • stud_issue_3.jpg
    stud_issue_3.jpg
    2.8 MB · Views: 68
  • stud_issue_2.jpg
    stud_issue_2.jpg
    3.1 MB · Views: 69
  • stud_issue_1.jpg
    stud_issue_1.jpg
    2.6 MB · Views: 80
Replies continue below

Recommended for you

@Tomfh I was lazy in my reply but his examples are generally on the ends of the walls
Here, the fixing pattern for the plasterboard has tighter spacing on the end stud so those compromised studs would be a PITA for the plasterboard fixers
Hence, I say replace those

Agree that the internal studs could just be doubled up
 
I agree with doubling up.

I also noticed the "T" posts look like they only have a block to nail to in the middle, none at the top and bottom. When did they start doing that?

There is no excuse for the one in the 4th picture. It should have been culled for sure.
 
Hi,

I am building a home with a builder and during the framing I found many studs that were cracked a lot. Builder pushed back on fixing these.
Need your input. Please see the attached pics. Like that there are several.
That is an issue and you need independent advice.

What country are you in?

You should be seeking a third party building inspector, engineer, or the appropriate person in your jurisdiction. In my jurisdiction I'd go with a reputable building inspector as they are likely less expensive, have a broader knowledge than a structural engineer and it doesn't take a genius to realise that those studs are non compliant. A structural engineer far better SPECIFIC knowledge regarding the structure, but a building inspector can look at everything more broadly.**

**This advice is most relevant in my jurisdiction. It may or may not apply in yours.
 
I agree those studs should be corrected.

My advice from my own experience building a home with a tract builder in the US:

Hire a "pre-drywall" home inspector. If the builder is allowing these studs to remain, there is no telling what other non-structural items may be non-compliant. I'd make time to walk through the home with your inspector to point out your areas of concern. Inform your builder that you have hired an inspector who will inspect the building PRIOR to drywall.

May be obvious, but also hire the inspector to do the final "pre-purchase" inspection prior to signing the final paperwork.
 