Jun 29, 2008 #1 civil75000 Civil/Environmental Joined Jun 29, 2008 Messages 1 Location US A stone yard needs to be “sprayed” or “tacked” down so the #304 remains in place. Anyone knows of a product what to use beside "tar & chip"? Thanks civil75000
A stone yard needs to be “sprayed” or “tacked” down so the #304 remains in place. Anyone knows of a product what to use beside "tar & chip"? Thanks civil75000
Jun 30, 2008 #2 coloeng Civil/Environmental Joined Apr 1, 2008 Messages 345 Location US You could try mag-chloride, it's used around here for dust control. Upvote 0 Downvote