I have an old drawing from the 50's of a vacuum tower that is carbon steel with a alloy liner on the inside of the shell. I know the liner is either 410S or 317 S.S. The liner is called out on the drawing as a 5/64" thk U.M. liner.

At this point I am not sure if the liner is Cladding, Weld Overlay or a sheet liner because I can only find a very few drawings for this item. What I would like to find out, if anyone knows, is what the U.M. stands for. Is anyone familiar with this abbreviation?
 
U.M is an old welding abreviation.

Don't remember what it stands for, just that it was welding.

Stands to reason with a vacuumn tower.
 
I believe the U.M. stands for Unmatched Material and also believe that this is a liner... but on your drawings do you show any welding symbols for this area... You can tell what the material is if you get a Third party Inspection Company that has a positive material Identification gun they will be able to tell you what the material composition is. I hope this helped
 
in the old days, was union melt, early submerged arc with bare wire /flux automatically fed.
 
would you have a loose liner on a vacuum column?
 
At this time the column is still in service. Will have to wait for the Turnaround to get inside and inspect. I suspect that what we have is weld metal overlay of some type won't know the exact material until we do PMI during turnaround. I did not mean to imply a loose liner but some of the Vac. columns have sheet liners that are plug welded to the shell and with a fillet around the O.S. edge of the sheet.

We are going to be installing several new nozzles in this column and I am just trying to prepare in advance of the TAR. I would like to avoid any surprises and was not familiar with this abbreviation. Thanks to those who responded.
 

5/64" thk. liner? Seems too thin for cladding or weld overlay. It's probably some kind of paintlike coating.
 