Experts,
Want to use MP35N for one component and the component needs to comply with NACE0175 and API 6A, and also satify structural analysis viewpoint. The material Spec I am thinking is:
min YS: 230 ksi
min TS: 240 ksi
min elongation: 15%
min RoA: 20%
min CVN at zero degree C: 20 ft-lb
max HRC: 51
Material will be cold-reduced and then 4 h aging at 704C(1300F). Is this possible? I am personally a bit concerned with elongation. Right now min YS is from my stress analysis, fixed; others are from those NACE and API standards, fixed also. I do have several more heat treatment options after cold-reducing as follow:
----------------------
Aging period, min Temperature
4 732C (1350F)
6 774C (1425F)
4 788C (1450F)
2 802C (1475F)
1 816C (1500F)
Can anyone recommend a heat treatment condition which will satify requirement?
Thanks a bunch
Salmon2
Want to use MP35N for one component and the component needs to comply with NACE0175 and API 6A, and also satify structural analysis viewpoint. The material Spec I am thinking is:
min YS: 230 ksi
min TS: 240 ksi
min elongation: 15%
min RoA: 20%
min CVN at zero degree C: 20 ft-lb
max HRC: 51
Material will be cold-reduced and then 4 h aging at 704C(1300F). Is this possible? I am personally a bit concerned with elongation. Right now min YS is from my stress analysis, fixed; others are from those NACE and API standards, fixed also. I do have several more heat treatment options after cold-reducing as follow:
----------------------
Aging period, min Temperature
4 732C (1350F)
6 774C (1425F)
4 788C (1450F)
2 802C (1475F)
1 816C (1500F)
Can anyone recommend a heat treatment condition which will satify requirement?
Thanks a bunch
Salmon2