I have my mitsubishi turbo 4g63 short block built with all the goodys. Ross,Scat,Clevite, ARP. My mains and rod beaings are at .0015- .0017 clearance after 10/10 on the crank and line hone. The factory specs ask for .0008- .0020 on both. I will be using royal purple 10/40 once the engine is broke in.
What are your thoughts on this seams tight to me???