Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

necking in tensile tesing 1

Status
Not open for further replies.

polybog

Materials
Jan 24, 2007
7
Dear all,

i am trying to simulate a tensile test. since in the real senario the material is anisotropic and in ansys i m modelling as isotropic (since i dont know all the matrix for anisotrory for my material). I am not able to get necking becoz of the isotropic property. Is there any other way to get the necking?

Regards
Polybog
 
Replies continue below

Recommended for you

The first method is to use two materials.
The necking part has a smaller E.

The second method is to make a small notch on the specimen.
Then, the deformation of the notch area will be larger than that of other part.


Notice: because the material is not linear elastic, the increment and the time during this simulation is impportant. Otherwise, there will be convergence problems, or the necking phenomenen will not be significant. If the increment is set small enough, you can can the same necking phenomenon with that of the experiment.

good luck!
 