NDEs for steam pipe

Status
Not open for further replies.

Davidorias

Industrial
Oct 22, 2002
26
Hello, I would like to know a NDE (Non Destructive Essay)for in-sevice steam pipe, 300ºC.

Thanks
 
Replies continue below

Recommended for you


To answer your question, a lot more information is needed. A comprehensive inspection program depends a lot on the physical characteristics and operational history of your plant.

I assume that this is a probably a carbon-steel steam piping system feeding a steam turbine or similar process component.

For a steam system of this type, both Ultrasonic testing and Radiographic testing are commonly used. In the USA, API-572(?) guideline has been used to set up inspection programs.

My opinion only....

MJC

 
Thanks, MJCronin. I have been reading an article about laser based nondestructive testing, named shearography. Probably is a very expensive technique, and is probably more addequate for very critical systems.
 