Does Section IX or D1.1 prevent the combining of multiple PQRs, one with PWHT and another without, from qualifying a WPS. A reference paragraph would be greatly appreciated.
A single WPS may cover
several essential variable changes as long as a supporting
PQR exists for each essential and, when required, supplementary