Feb 15, 2023 #1 Uralsk Mechanical Joined Feb 21, 2021 Messages 39 Location ID What is the best way to melt down metal that has 3000° degree celsius melting point at medium scale backyard foundry
What is the best way to melt down metal that has 3000° degree celsius melting point at medium scale backyard foundry
Feb 15, 2023 #2 bobjustbob Materials Joined Feb 8, 2017 Messages 149 Location US There is no way you are getting to 3000°C. You are not getting to 3000°F in a backyard foundry. Bob Upvote 0 Downvote
Feb 15, 2023 #3 EdStainless Materials Joined May 20, 2004 Messages 16,345 Location Waukesha WI USA Build an arc furnace? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
Build an arc furnace? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Feb 15, 2023 #4 Metalfixer Mechanical Joined Sep 8, 2003 Messages 112 Location US https://www.theatlantic.com/technol...wered-furnace-can-reach-3-000-degrees/360423/ Upvote 0 Downvote