Suggest you contact the technical folks at Special Metals, but I think you could use (1)82 or Inco A.
 
Sorry you did say GMAW, ERNiCr-3 ( 82) should work.
 
There are a number of nickel base weld filler metals that can be used. You need to determine the corosion compatabilty of the materials before selecting the appropriate one.

 