Jul 17, 2005 #1 GrzegorzD Mechanical Joined Apr 1, 2003 Messages 28 Location PL Hello, If anybody know the modulus of Elasticity for Bolt M14x1.5 10.9 and steel tube E235 +C (EN 10305-1:2002) or St35BK (DIN 2391-2) Thanks
Hello, If anybody know the modulus of Elasticity for Bolt M14x1.5 10.9 and steel tube E235 +C (EN 10305-1:2002) or St35BK (DIN 2391-2) Thanks
Jul 18, 2005 #2 EdStainless Materials Joined May 20, 2004 Messages 16,381 Location Waukesha WI USA Room temp values plain carbon, low carbon steel 27.9ksi plain carbon, high carbon steel 29.9ksi (the breakover is about 0.30-0.35% C) alloy steels, high carbon (4140, 4335) 31.6ksi These are from the ASM book on high temperature properties of ferrous alloys. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm Upvote 0 Downvote
Room temp values plain carbon, low carbon steel 27.9ksi plain carbon, high carbon steel 29.9ksi (the breakover is about 0.30-0.35% C) alloy steels, high carbon (4140, 4335) 31.6ksi These are from the ASM book on high temperature properties of ferrous alloys. = = = = = = = = = = = = = = = = = = = = Corrosion never sleeps, but it can be managed. http://www.trenttube.com/Trent/tech_form.htm
Jul 18, 2005 Thread starter #3 GrzegorzD Mechanical Joined Apr 1, 2003 Messages 28 Location PL Thanks a lot GrzegorzD Upvote 0 Downvote