Any thoughts on what is the best way to model an OSB panel? I am modelling a roof with rafters and OSB on top therefore i would like to add the OSB sheathing on my analytical model.
I am thinking of using the the following element
1. Shell elelement -> Orthotropic
Youngs modulus in x direction, Ex = 11000 MPa
Youngs modulus in y direction, Ey = 11000 MPa
2. Thickness = 18mm
3. Material = timber
Any idea what values shall i use for Youngs Modulus?
UPDATE:
The values to be used for the youngs modulus for OSB3 are
Youngs modulus in major axis = 3500 N/mm2
Youngs modulus in minor axis = 1400 N/mm2
I am thinking of using the the following element
1. Shell elelement -> Orthotropic
Youngs modulus in x direction, Ex = 11000 MPa
Youngs modulus in y direction, Ey = 11000 MPa
2. Thickness = 18mm
3. Material = timber
Any idea what values shall i use for Youngs Modulus?
UPDATE:
The values to be used for the youngs modulus for OSB3 are
Youngs modulus in major axis = 3500 N/mm2
Youngs modulus in minor axis = 1400 N/mm2