I need help as to what super plasticizer to use on landscaping curb, the mix is 4each 5 gal bucket sand to 47lbs Portland with fiber added should give me around 3200 psi. This mix is close to zero slump I live in Indiana and freeze and thaw on the finished curb will apply and I need a smooth finish so time to work with mix is very important. If any one could recommend what admixes to use. Thanks for any help
 
More importantly, you need air entrainment admix AEA. Your low slump is OK, but you might consider sawcutting the curbs approx 6 to 8 hours after they are case... Superplasticisers are specific to the product and you would have to talk to the supplier.

Dik
 
Thanks dik for the info. The curb will be formed buy a landscape curbing machine and control joints cut every 2’ after we lay the curb trowel and stencil.

The mix:
4 each 5gal buckets mortar sand and 47lbs Portland. This will be mixed at job site.
Fiber added.

I need to add strength and curing time for finish toweling to achieve a smooth finished curb, I have read that some are using a spray after the curb is down to achieve a smooth finish? What would they be using to do this with? Any help!

I would like to prefect this mix to ease the working of the curb and finish (troweling and stamping)
 
By fibre, I assume you are using polypropylene... I'm not sure this will be effective. You don't seem to mention any coarse aggregate; I would think that you would have some 3/4" stone. The sand only would make it more difficult to have any freeze thaw resistance without compromising the strength. You need a good mix, probably about 35 MPa, and about 7% air. Slump should be limited to about 3" maximum.

Mix design is closely tied into the local aggregate; it has an effect on the moisture conditions of the material that you are using. You'd be best served by talking to a local concrete contractor or concrete supplier. I can produce a concrete design and even locally, it would have to be 'tuned' to suit.