commandotom
Materials
Hello. I was hoping someone might be able to help me out.
I've completed doing an API510 inspection for a customer. From the U-1;
The vessel (1966) fabricated from SA264 (1/16th 316L on SA212-B backing)
MAWP=100psi @ 600F, Dia.=96", Crown Radius=84", Knuckle Radius=6.5"
Bottom Head 0.496", Top Head 0.410
Allowable Stress for Mat'l= 17500; Efficiency=0.85
Assumed; Torisphereical Heads (no Drawings)
When I crunch the numbers for min "t" I get 0.500"
So the thickness specified for the heads is less than the calculated value.
What am I missing? I don't have access to the Code for that period.
Just want to be able to explain to the customer what is going on here.
Suggestions??
As always thanks in advance.
I've completed doing an API510 inspection for a customer. From the U-1;
The vessel (1966) fabricated from SA264 (1/16th 316L on SA212-B backing)
MAWP=100psi @ 600F, Dia.=96", Crown Radius=84", Knuckle Radius=6.5"
Bottom Head 0.496", Top Head 0.410
Allowable Stress for Mat'l= 17500; Efficiency=0.85
Assumed; Torisphereical Heads (no Drawings)
When I crunch the numbers for min "t" I get 0.500"
So the thickness specified for the heads is less than the calculated value.
What am I missing? I don't have access to the Code for that period.
Just want to be able to explain to the customer what is going on here.
Suggestions??