sdz
If the loads are much less than cracking moment (ie acceptable as a plain concrete member) i would just provide minimum temperature and shrinkage reinf. bearing in mind the degree of restraint (if any) and that for members greater than 500 thick, reinf. can be calculated for D=250mm (to each surface).
Cheers