Mar 22, 2011 #1 Downhand Industrial Joined Dec 20, 2009 Messages 59 Location CA B31.3 331.1.3 says that heat treatment is required when the thickness through the weld in any plane is greater than twice the minimum material thickness requiring heat treatment. What is minimum material thickness referring to?
B31.3 331.1.3 says that heat treatment is required when the thickness through the weld in any plane is greater than twice the minimum material thickness requiring heat treatment. What is minimum material thickness referring to?
Mar 22, 2011 2 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US The minimim base material thickness refers to the nominal wall thickness for thermal treatment in Table 331.1.1 for stated base materials. Upvote 0 Downvote
The minimim base material thickness refers to the nominal wall thickness for thermal treatment in Table 331.1.1 for stated base materials.