Can anyone recommend an alterantive metal to tantalim for boiling mixtures of HCl from 1 to 20 %.

We currently use various grades of hastalloy but they tend to suffer corrision and fail within 2-3 years life span.

Obviously you can use plastics but the tend to not be as strong. Our temps go up to 180°C and in some applications to 230 deg C
 
You're getting close to needing Au or Pt!
 
I believe Zr can be used in these conditions - you can get information from Wah Chang at:



Regards,

Cory