I've been unable to find any tensile and yield strength listed for this alloy and temper of aluminum.

can anyone point me in the right direction?????
 
Replies continue below

Recommended for you

From the ASM metals handbook desk edition:

For extruded wire, bar, rod, or shapes:

6105-T5 -- for dia up thru 12.70mm; Min UTS: 262MPa Yeild: 241 MPa ; min elong: 10%.



 
The minimum values NickE stated are also good up to 1 inch, per ASTM B221.
 