RAJMETALLURGY
Materials
Material: G18NiMoCr3-6
Test coupon thickness 172 mm, length 200 mm and width 122.5 mm.
Is it possible to achieve the tensile and impact properties as below,
Impact @ -40 Deg C: 27 Joules
YS: 760 MPa min
UTS: 900 MPa min
%E: 12% min
%R: 25% min.
Please comment on this.
Test coupon thickness 172 mm, length 200 mm and width 122.5 mm.
Is it possible to achieve the tensile and impact properties as below,
Impact @ -40 Deg C: 27 Joules
YS: 760 MPa min
UTS: 900 MPa min
%E: 12% min
%R: 25% min.
Please comment on this.