hi,
i need to measure the wall thickness of a certain product , the product is made of ceramics and has an egg like shape which makes it very difficult to measure, in addition the wall thickness is not constant and varies along the profile . the average wall thickness is about 8.5 mm.
i tried using standard mechanical measuring tools (all sorts of big calibers and similar methods) , an ultrasonic gauge and i even found a kind of magnet based gauge but they all have the same problem- not accurate enough, i need an accuracy of at least +- 0.01 mm , if anyone has an idea on how to do it id love to hear it.
thanks
i need to measure the wall thickness of a certain product , the product is made of ceramics and has an egg like shape which makes it very difficult to measure, in addition the wall thickness is not constant and varies along the profile . the average wall thickness is about 8.5 mm.
i tried using standard mechanical measuring tools (all sorts of big calibers and similar methods) , an ultrasonic gauge and i even found a kind of magnet based gauge but they all have the same problem- not accurate enough, i need an accuracy of at least +- 0.01 mm , if anyone has an idea on how to do it id love to hear it.
thanks