Welded with A 106 grade B material witha 6010 root and 7010 and 7018 fill/cap, based on tensile strenght of electrode and materials, let me know if I'm correct, this qualifies:
1. P1 group 1,2,3 materials right? although group 3 is 70k material, charpy impast testing is not required, so I'm thinking it can be welded with the WPS
2. API 5L X-42, X-46, X-52 materials too since they're all under 70k of tensile right?
3. Finally, in the PQR the actual p1 group 1 to p1 group 1 was specified, but the in WPS, I can simply put P1 to P1, or do I have to specify group 1,2&3 to group 1,2&3 too?
Thanks you.
Welded with A 106 grade B material witha 6010 root and 7010 and 7018 fill/cap, based on tensile strenght of electrode and materials, let me know if I'm correct, this qualifies:
1. P1 group 1,2,3 materials right? although group 3 is 70k material, charpy impast testing is not required, so I'm thinking it can be welded with the WPS
2. API 5L X-42, X-46, X-52 materials too since they're all under 70k of tensile right?
3. Finally, in the PQR the actual p1 group 1 to p1 group 1 was specified, but the in WPS, I can simply put P1 to P1, or do I have to specify group 1,2&3 to group 1,2&3 too?