Jul 1, 2002 #1 jmcgrath Petroleum Joined Jun 6, 2002 Messages 29 Location GB Dear All, I am looking for a material that will bond to carbon steal to create a coating what will be very resistant to abrasion and will insulate the metal electrically. Does anyone have any suggestions? Thanks, John McGrath
Dear All, I am looking for a material that will bond to carbon steal to create a coating what will be very resistant to abrasion and will insulate the metal electrically. Does anyone have any suggestions? Thanks, John McGrath
Jul 1, 2002 #2 GRoberts Materials Joined Apr 22, 2002 Messages 548 Location US There are various types of epoxy paints that would probably meet your needs. Your best bet would be to talk to a coating supplier. Upvote 0 Downvote
There are various types of epoxy paints that would probably meet your needs. Your best bet would be to talk to a coating supplier.
Jul 1, 2002 #3 tomwalz Materials Joined May 29, 2002 Messages 947 Location US You can braze various ceramics to steel. Tom Upvote 0 Downvote
Jul 8, 2002 #4 dsherf Materials Joined Jul 2, 2002 Messages 1 Location IL John you have a good option by choosing dry lubricants as like epoxy mix with MoS2. Danny Upvote 0 Downvote
Jul 15, 2002 #5 gdodd Automotive Joined Jul 18, 2001 Messages 138 Location AU PVD applied coating such as TiN TiCN or CrN are wear resistant, oxidation resistant and being a ceramic coating, electical insulators. Upvote 0 Downvote
PVD applied coating such as TiN TiCN or CrN are wear resistant, oxidation resistant and being a ceramic coating, electical insulators.