Hello ,
I was checking whether you guys have material properties for Nordam panels NL 610-10777-375 & NL 610-11233-375

Let me know guys if any one of you have allowables and source of same.

Please advice.

Kakalip
 
Replies continue below

Recommended for you

Nordam should provide the data to you.

Wes C.
------------------------------
No trees were killed in the sending of this message, but a large number of electrons were terribly inconvenienced.
 
I asked them but particular said that it was not with them at moment.
 
Nordam should be able to provide you with something! at the very least the;
Long Beam Flexure, “L” Direction Skin Stress, psi
and Climbing Drum Peel in-lb/3-inch width

I have got some specs out of them for 610-10233-500 and similar but not the numbers you quoted, they are pretty slow at getting info to you in my experience.

If you were supplied with the actual panels I would be jumping up and down a bit more :)
 