We are applying a .050" THK Ni-5%Al HVOF coating on a structural component & require to establish various design criteria & require the material properties for this "sintered" material. Would anyone have data sheets on HVOF applied Ni-5%Al material?

In particular we require ultimate / yield / elongation / poisson values / etc. (finite element requirements).. should this not be possible - what is the most comparable substance? Would a 95% pure sintered Ni be comparable to an annealed Nickel 200 ??? any ideas ?
 