Does anyone have an opinion concerning the neccesity for magnetic flux leakage testing of fired heater tubes which in all respects comply with the standard requirements of ASTM A-335 Gr P91? The tubes (pipe) are nominal 6 inch diameter, Sch. 40 and were hydrotested at the mill to 2800 psi. Tube metal temperatures are 975F and 1200F.
If anyone has experience to indicate that MFL testing is a requirement is there an acceptable alternative test that can be performed?
If anyone has experience to indicate that MFL testing is a requirement is there an acceptable alternative test that can be performed?