The information on lubrication of stainless screws was very informative. I have a question as to turning components. Close tolerance with a gap of 0.0003". At temperatures up to 600 deg. F, would the same lubricating materials be useful? Or would a coating such as Titanium disulfide be a good match. What are your thoughts?