Mar 18, 2003 #1 axial Mechanical Joined Feb 25, 2002 Messages 13 Location US Can someone tell me if a bolt is considered lubricated if it has a zinc dichromate finish applied to it
Can someone tell me if a bolt is considered lubricated if it has a zinc dichromate finish applied to it
Mar 18, 2003 #2 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US No, the bolt would not be considered lubricated. There are polymer topcoats that are added over electroplated zinc coatings (with or without chromate conversion coatings) that are used to lubricate bolts. Upvote 0 Downvote