Hello All,

Is there any low temperature processing technique by which one can fabricate ceramic with high mechanical strength? For example I have alumino-silicate crystals with avg. crytsal size of 300 nm, shaped to green body and the limit of temperature for processing is 900 °C.

I am trying to use amorphous silica with 40 nm particle size and then sintered it to 900 °C but results are not good. Does someone know what is melting point curve of silica/alumina with particle diameter?

Thanks
 
how high is high? Geopolymers can be constructed with "high " strength at temperatures below 100 C. May need to add fibers for notch toughness . Reports are that China is using Geopolymers for the ablative coating of their space shuttle.

"Nobody expects the Spanish Inquisition! "
 
sintering temperature can go up to maximum 900 °C. and the temperature for normal operating use is 500 °C maximum!
 
Have you considered:

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529
 