I am making a glass filled PET compound on a twin screw extruder. Properties are good except for an extremely low HDT value of approx 80 C instead of 215 which commercially available grades have. I still get this low number even when I use an alternative grade of PET. Strand length in the compound is good, no excessive breakage.

Does anyone have any ideas on how to improve this property?
 
Replies continue below

Recommended for you

80 deg C is a low HDT for PET, even unfilled. Are you useing homopolymer or copolymer, is it crystalised or amorphous. is it PETG.

Many beverage bottle compounds are amorphous copolymer.

Are you useing a glass fibre with good aspect ratio and suitable surface coating or sizeing agent

Regards
pat
 