Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for material aisi 4145 and aisi4145H standard mechanical properties

Status
Not open for further replies.

ra11231

Mechanical
May 31, 2019
1
I was looking for AISI 4145 and AISI4145H Material data, please help me out if any one has the standadrd document(ams,astm,etc..)
 
Replies continue below

Recommended for you

It is not that simple. The mechanical properties in specifications are based on product form and heat treatment. Thus, you will see different properties in different standards. If you are designer, then you may want to look in the ASME Boiler & Pressure Vessel code after you determine the applicable spec to find design allowable stresses for your application in the Materials section.
 
ASM Handbook.
Google.
Supplier data sheets.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
the only difference between the two is that the H has restricted hardenability, a narrower scatter on a Jominy test bar.
There are some good producer data sheets that will show the relationship between temper temperature, strength, and toughness.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
I see Matweb still cannot spell phosphorus.