Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations dmapguru on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Looking for 2 EN metal casting standards 1

Status
Not open for further replies.

tgeorge7435

Mechanical
Joined
Dec 5, 2006
Messages
1
Location
US
I would appreciate information on the closest EN standards in terms of chemistry and mechanical properties to the following ASTM standards. I realize the equivalence may not be exact particularly in the mechanical certification tests.

The ASTM standards are castings and are:
A 351 grade CF8M
and A 216 grade WCB

Thanks,
 
As per ASM Heat Treater's Guide (2nd edition, page 795):
ASTM A351, grade CF8M is type 316 Stainless Steel. The chemical composition is:
0.08% C, 1.50% Mn, 2.00% Si, 9.0 to 12.0 % Ni, 18.0 to 21.0% Cr, 2.0 to 3.0% Mo.

Rao Yallapragada

Rao Yallapragada
 