Hi forum members
Reference: ASME B 31.3 chapter IX, table k-1, allowable stresses in tension for metals for chapter IX.
Material spec. API 5L Gr x42 to x80.
Note 6: this type or grade is permitted only in the seamless condition.
Query
1) For high pressure piping chapter IX of ASME B31.3, code restrict usage of seam-welded API 5L spec pipe. But why such limitation.
2) if such restrictions are to be overlooked what necessary precautions shall be taken(change in API 5L spec./ other technical ).
Thanks in advance
P.S changed query number 2 after looking at first answer
Reference: ASME B 31.3 chapter IX, table k-1, allowable stresses in tension for metals for chapter IX.
Material spec. API 5L Gr x42 to x80.
Note 6: this type or grade is permitted only in the seamless condition.
Query
1) For high pressure piping chapter IX of ASME B31.3, code restrict usage of seam-welded API 5L spec pipe. But why such limitation.
2) if such restrictions are to be overlooked what necessary precautions shall be taken(change in API 5L spec./ other technical ).
Thanks in advance
P.S changed query number 2 after looking at first answer