I have a general question. I have a building that has a 6'-0" high above finish floor 8" thick concrete wall around the entire perimeter. The wall varies from 3'-0" to 6'-0" below finish floor for frost protection and height at the loading dock. So the wall varies to between 9'-0" to 12'-0" in total height. My question is how often should I place expansion joints in this wall?
thanks.
 
Replies continue below

Recommended for you

Depends on the overall size of the wall.

Is it reinforced or plain concrete?
 
Expansion joints or control joints? I would say expansion joints every 200', control joints every 12-16'. Anyone disagree?
 
It is an addition and the front and rear walls are 150'-0" long while the side wall is 300'-0" long. It is reinforced. I am talking expansion joints. I have the control joints located at no more than 1.5 times the wall height and closer to 1.0.
 
I see no reason for an expansion joint in a 300' long concrete wall, unless there is an expansion joint in the building. Concrete shrinks so contraction is the issue.
 
rowing,

That is a good link. I have always used technical report 65 for placing thermal expansion joints. However, I have never made the interpretation with regards to option #3. I have always tried to limit my lengths to around 400-500 feet (and I thought that was pushing it). However, according to option #3 I could go as much as 800 feet as long as my bracing is in a side.... I'm not entirely sure I am comfortable with that.
 
Thanks for all your help. All the replies were very helpful. I enjoyed receiving your good advice. I guess I was a little too conservative. Kinda like the old engineer I knew that wore a belt and suspenders.
 