Laser Welding of 304L Stainless Steel

Status
Not open for further replies.

BATman2

Mechanical
Mar 22, 2002
43
I have a supplier that is proposing to change a large spot welded structure to laser welded. Structural issues aside, does anyone have any experience with volumetric inspection of laser welds (excluding x-ray)? Any suggestions on how to go about that? The sample provided to me shows a very narrow weld "line", ultrasonic inspections would be difficult I think.

Thanks,
Batman2
 
Replies continue below

Recommended for you

You have hit on the issue, the weld width and volume is very small. You could use UT, but you might find yourself rejecting on minor variations not related to fusion.

= = = = = = = = = = = = = = = = = = = =