Lasering Galvanized 12gauge with 7 lens on a Mitsubishi lazer 3015ex what settings can I use thx.
 
You should have a book or pdf with cut conditions.
SECN7 or maybe GALV7
 
thx for the help but no pdf or book . the book itself tell you how to adjust it but dose not give a condition to start .Iam working from scrath can I use a amada setting seems that averyone uses those.
 
I can check our conditions but you need to cut it with nitrogen or shop air. You get poisinus gas if you cut with oxygen.
 
I can use shop air thx
 
we also have nitrogen . thx for your help .If iam close I can adjust also I am using 7.5 len sorry but I do have 5 lens .
 