Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Laser pre-treatment instead of grit blasting prior to thermal spray coating

Status
Not open for further replies.

Feldmann359

Industrial
Joined
Jun 9, 2009
Messages
28
Location
DE
Hello Colleagues,

In advance of a thermal spray coating process, a sand blasting
with abrasive grit material (e.g. corrundium) is required
to reach a sufficient bonding strength of the coating.

The grit blasting process leads to embedding of grit into the substrate as well as to small micro-cracks which could be detected by sectioning and subsequent microscopy.

In my case, embedding of contaminants should be avoided.

Does somebody know wheter it is possible to use a laser surface
process instead of grit blasting to increase the substrate surface area? My substrate does not form a passivation scale.

Thanks a lot
Feldmann






 
It may be possible to use a laser pretreatment. CleanLaser is one equipment provider for this.
 