Does anyone have some suggestions on cutting 1/2" corian material. I'm using a 2000w Mitsubishi. Have cut many materials but this is a first. Any help would be appreciated
 
Replies continue below

Recommended for you

hello

corian is an "homogenuous" mix between 1/3 PMMA and 2/3 ATH
I think you can try your PMMA parameter

The pooh
 
Hello thepooh.


What is ATH? Do you know the exact formula of corian?

Best Regards..
 
ATH means in French "trihydrate d'alumine "
it's like bauxite / the mineral base of aluminium

I don't know the exact formula of Corian : it's a patented
material of Dupont/Zodiac

Happy Xmas and happy NewYear
 