i will shortly be involved in the testing of some Very sour oil samples at reservoir temperatures and pressures. I would be interested in any advice you could provide on the suitability of 316 Stainless pressure vessels and tubing.
As a guide the rough test parameters are given below
Pressure 0 to 15000psig
temperature ambient to 200 degrees C
expected residence time in equipment 12 hrs
H2S levels upto and Beyond 600ppm.
thank you
As a guide the rough test parameters are given below
Pressure 0 to 15000psig
temperature ambient to 200 degrees C
expected residence time in equipment 12 hrs
H2S levels upto and Beyond 600ppm.
thank you