Zylinderkopf
Mechanical
Greetings to all:
I am re-posting this question in your forum as the AWS Forum did not have any visitors that elected to respond to it - - my error.
Our refinery has a an ASME B31.3 Pipe Specification with the particulars included below.
I can not seem to verify the reasoning behind this Specification's existing requirement for PWHT (could it possibly be some sort of H2 bake-out?).
Otherwise, maybe there should not be a PWHT requirement in this case (all pipe and appurtenances covered by this spec are P1 material).
As such, if anyone could share with me an informed judgement as to whether PWHT is / is not a valid requirement in this case then I will remain grateful.
Thank you all (again) for your time and kind consideration of my enquiry.
- - Pipe Specification Particulars - -
Material: Carbon Steel (pipe utilizes ASTM A106 Grade B CS)
Pressure / Temperature Limitations: ASME Class 600
Service: Hydrocarbon with > 100 PSIA H2 Partial Pressure
Minimum Corrosion Allowance: 0.050"
I am re-posting this question in your forum as the AWS Forum did not have any visitors that elected to respond to it - - my error.
Our refinery has a an ASME B31.3 Pipe Specification with the particulars included below.
I can not seem to verify the reasoning behind this Specification's existing requirement for PWHT (could it possibly be some sort of H2 bake-out?).
Otherwise, maybe there should not be a PWHT requirement in this case (all pipe and appurtenances covered by this spec are P1 material).
As such, if anyone could share with me an informed judgement as to whether PWHT is / is not a valid requirement in this case then I will remain grateful.
Thank you all (again) for your time and kind consideration of my enquiry.
- - Pipe Specification Particulars - -
Material: Carbon Steel (pipe utilizes ASTM A106 Grade B CS)
Pressure / Temperature Limitations: ASME Class 600
Service: Hydrocarbon with > 100 PSIA H2 Partial Pressure
Minimum Corrosion Allowance: 0.050"