Pls go through SE-747 for "MATERIAL GROUPING CLASSIFICATION OF WIRE IMAGE QUALITY INDICATORS (IQI) USED FOR RADIOLOGY"
As per SE-747,Materials have been designated in eight groups based on their radiographic absorption characteristics:groups 03, 02, and 01 for light metals and groups 1 through 5 for heavy metals.And as per Materials Group 1: Image quality indicators (IQIs) shall be made of carbon steel or Type 300 series stainless steel.
My conclusion is that "SS" and "Fe" IQI in RT is not that much significant difference .And availability of "SS" wire IQI is only for extensive application and not for any 'code' requirments.