Hello all,

I have a scenario in which I am tapping m10x1.5 threads into cast iron close to an edge - ~0.120". (imagine a 2x2 that is 6 inches long, with a hole drilled in the end faces off-centered such that the edge of the hole is .120" from the sides).

This distance should not move - it's pretty darn controlled dimensionally.

I am a touch worried about the small remaining wall thickness... I know that there are a few "rules-of-thumb" out there with respect to minimum distance to edge, but they are not always practical and arguably excessive. However, how would I quantify the local peak stresses I would see in the internal threads with a engaged thread length of about 20 mm? these are metric threads so there is no radius callout at the root of the thread, so I'd have to assume something geometrically... :(

I have tried using FEA, but it's not very clean at all, as you can imagine (levels around 400 ksi σ1 but I am fairly convinced these are just singularities)....

Anyways, any suggestions to what ails me above?

TIA!
 
Replies continue below

Recommended for you

Loading from tightening, side loading the bolts into the thin edge, ??
 
Hi Tmoose,
I suppose I should have specified. There’s really no way for side loading to occur in this joint - the clamp load should provide plenty of resistance to slipping/subsequent bolt/thread moments occurring . It would be nice to be able to quantify somehow, but not the priority. So I would mainly say the loading from torque, and that loading from torque is also what I “attempted” to simulate. Thanks!
 