Insulation of Heated Bafffles

Status
Not open for further replies.

LarHanly

Mechanical
Jul 5, 2017
1
Hi,

I have created a pair of baffles to restrict the airflow in a polymer extrusion process as shows in the image.
I wish to insulate these baffles in the area shown so that any heat conducted from the die piece is directed inwards.
Could someone please suggest a product such as a stick on insulation tape which could be used here?
Baffles_z7pqhk.png


Any help would be greatly appreciated.
Alos please let me know if there is another forum which would prove more suitable
Kind Regards
 
Replies continue below

Recommended for you

A bit of a lash-up, but try wrapping several layers of aluminium foil around -secure with copper wire.

www.tynevalleyplastics.co.uk

Politicians like to panic, they need activity. It is their substitute for achievement.
 