Can anyone provide guidance to the use of a 6061-T6 aluminum rivet? We have a customer who has trouble installing (not holding in place). Our customer supplied the drawing, which specifies a shank diameter of 0.576-0.595. We do not know the actual hole size, but believe they may have a larger hole size that is causing the problem. The shank diameter is unusual (small) for a "5/8" rivet. Can 6061 rivets be installed when they are in the T6 condition?