Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Inspection Method

Status
Not open for further replies.

HectorMontalvo

Industrial
May 22, 2003
5
Hi, i would like to know if somebody meets any kind of test or process to find out some kind of pourisity into the finished carbon steel?
 
Replies continue below

Recommended for you

Hope you mean porosity in carbon steel and not pourisity because I don’t think any thing like that exist in carbon steel.
If you mean porosity in carbon steel, the following tests can be carried out to determine porosity in carbon steel.
(1) Ultrasonic Testing: a non destructive test that enables typical metal (Carbon steel) faults like cracks, blow holes and inclusions to be detected and located. It works through the same mechanism of echo sounding device in ships . Information revealed can be viewed on a CRT (cathode ray tube).
(2) Radiographic Techniques : examples of this techniques are X-ray and Gamma ray techniques.They can also be used in detecting and locating porosity in metals.
(3) Dye- penetrant testing: this test is suited only to the detection of various types of surface defects like grinding and fatigue cracks,porosity and lack of joint welds.
 