May 1, 2024 #1 jafary64 Mechanical Joined Nov 12, 2009 Messages 35 Location US Hi my friends we Have a Spiral wound Gasket Without inner ring then I want to know 1- is this material manufactured by standard and what is the standard 2- when can use this material according to standard thanks a lot
Hi my friends we Have a Spiral wound Gasket Without inner ring then I want to know 1- is this material manufactured by standard and what is the standard 2- when can use this material according to standard thanks a lot
May 1, 2024 #2 GBTorpenhow Mechanical Joined Jan 26, 2022 Messages 267 Location US Is there an outer ring? Any markings? Upvote 0 Downvote
May 3, 2024 #3 david339933 Industrial Joined Jun 15, 2011 Messages 1,204 Location CA ASME B16.20. You know you could find that in 5 seconds on google. Upvote 0 Downvote