Nov 21, 2014 #1 tekari123 Mechanical Joined Aug 7, 2013 Messages 29 Location IN Dear All, In which case the ''Induction Heating'' of piping components are mandatory over ''Resistance Heating''?? Is there any code reference or bindings..? Thanks in advance, Alok
Dear All, In which case the ''Induction Heating'' of piping components are mandatory over ''Resistance Heating''?? Is there any code reference or bindings..? Thanks in advance, Alok
Nov 22, 2014 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US None that I can think of in US codes and standards. This is a process detail, or decided by the owner/user of engineering firm. Upvote 0 Downvote
None that I can think of in US codes and standards. This is a process detail, or decided by the owner/user of engineering firm.
Nov 24, 2014 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,809 Location US Ditto metengr, none in the USA. Upvote 0 Downvote
Nov 29, 2014 #4 CarlosVega Petroleum Joined Nov 29, 2014 Messages 2 Location MX None in ASME Code. Is a decision of User or Client. Upvote 0 Downvote