Hi everyone.
This is one simple question but was challenged, hope I can get support herein.
For pipeline induction bend, we usually use 3d (12” above) or 5d (less than 12”) as governing for curvature radius, it actually can facilitate the pigging during erection and operation. I believe such practice must be followed in most engineering design firm.
However, when we review one of pipeline design in which around 2km pipeline are set on jetty and trestle, 1.5d induction bend is provided for the 14” line due to restricted jetty spacing as explained. We were going to advise a higher curvature radius, e.g. 3d, as mandatory comment to be incorporated, unfortunately the stakeholder doesn’t like to revise his design and wonder which code the “3d” curvature radius was specified in.
Honestly speaking, I didn’t find code basis from ASME or API, even in design manual that I own. Can anybody herein guide me for code support? Or was I really wrong that 1.5d can be applied for pipeline with pigging requirement?
Thanks.
This is one simple question but was challenged, hope I can get support herein.
For pipeline induction bend, we usually use 3d (12” above) or 5d (less than 12”) as governing for curvature radius, it actually can facilitate the pigging during erection and operation. I believe such practice must be followed in most engineering design firm.
However, when we review one of pipeline design in which around 2km pipeline are set on jetty and trestle, 1.5d induction bend is provided for the 14” line due to restricted jetty spacing as explained. We were going to advise a higher curvature radius, e.g. 3d, as mandatory comment to be incorporated, unfortunately the stakeholder doesn’t like to revise his design and wonder which code the “3d” curvature radius was specified in.
Honestly speaking, I didn’t find code basis from ASME or API, even in design manual that I own. Can anybody herein guide me for code support? Or was I really wrong that 1.5d can be applied for pipeline with pigging requirement?