Dear all,
I have come across a typical requirement form one customer to include Solution Annealing activities of existing pipeline before cutting the same for any modification. The intended purpose is to prevent any crack from being propagated during cutting operation, as per customer. The metallurgy is SS321H, 30" NB, operating temperature is 600+ deg C, likely cyclic service. We need to take a tapping in the existing header and replace a portion of the 30" header. The line is part of the inlet line to the Catofin reactor in an MTBE plant.
I have already exhausted the limited resources, I had, but could not find any such requirement or reference for the same. My specific questions are:
1. Whether there is any requirement of Solution Annealing or any other heat treatment for existing pipeline, before doing any cutting operation.
2. IS it possible to carry out solution annealing at site on existing pipeline (on elevated structure)?
3. Does anyone have any experience of such an activity, or is there any reference material (codes/standards etc) where such requirements are mentioned?
Would really appreciate any fruitful response from members, before I go back to client to ask where are they coming from on this?
Thanks and best regards,
Niladri
I have come across a typical requirement form one customer to include Solution Annealing activities of existing pipeline before cutting the same for any modification. The intended purpose is to prevent any crack from being propagated during cutting operation, as per customer. The metallurgy is SS321H, 30" NB, operating temperature is 600+ deg C, likely cyclic service. We need to take a tapping in the existing header and replace a portion of the 30" header. The line is part of the inlet line to the Catofin reactor in an MTBE plant.
I have already exhausted the limited resources, I had, but could not find any such requirement or reference for the same. My specific questions are:
1. Whether there is any requirement of Solution Annealing or any other heat treatment for existing pipeline, before doing any cutting operation.
2. IS it possible to carry out solution annealing at site on existing pipeline (on elevated structure)?
3. Does anyone have any experience of such an activity, or is there any reference material (codes/standards etc) where such requirements are mentioned?
Would really appreciate any fruitful response from members, before I go back to client to ask where are they coming from on this?
Thanks and best regards,
Niladri