I was able to access a copy of B31.5, and there is specific reference to ASME Section VIII, Div 1, Part UG, UG-84 for impact testing. There is one caveat, you need to review 523.2.2. Instead of following UG-84 completely, there is a substitution for UG-84 (b)(2).