The ASME codes talk about impact testing being required for temperature below -20°F unless you de-rate the material. However, it does not say whether or not the welds are subject to impact testing.

Steve Mackie
Halifax, NS
 
packie81, apparently you are concerned with CS materials, if so, see UCS-67.

Regards,

Mike
 
But does UCS-67 also apply to welds made under B31.5?

Steve Mackie
Halifax, NS
 
I was able to access a copy of B31.5, and there is specific reference to ASME Section VIII, Div 1, Part UG, UG-84 for impact testing. There is one caveat, you need to review 523.2.2. Instead of following UG-84 completely, there is a substitution for UG-84 (b)(2).
 